Nur Azizah Affandy
Departement Civil Engineering, Faculty of Sains and Technology, Universitas Islam Lamongan, East Java 62211, Indonesia Indonesia
Muhammad Yaafi’ Ikbar
Departement Civil Engineering, Faculty of Sains and Technology, Universitas Islam Lamongan, East Java 62211, Indonesia Indonesia
Sugeng Dwi Hartantyo
Departement Civil Engineering, Faculty of Sains and Technology, Universitas Islam Lamongan, East Java 62211, Indonesia Indonesia
Data Iranata
Departement Civil Engineering, Faculty of Civil, Planning, And Geo-Engineering, Sepuluh Nopember Institute of Technology, East Java 60111, Indonesia Indonesia
Keywords: Compressive strength, concrete, HDPE, naphthalene-based superplasticizer, workability
ABSTRACT
The accumulation of plastic waste has encouraged the development of sustainable concrete using recycled materials. This study evaluates the use of High-Density Polyethylene (HDPE) waste as a partial replacement for fine aggregate in low-strength concrete incorporating a naphthalene-based superplasticizer. HDPE was introduced at replacement levels of 0%, 5%, 10%, and 15% by weight of fine aggregate, while the superplasticizer dosage was fixed at 0.5% by weight of cement. Workability was assessed using a slump test, and compressive strength was measured at curing ages of 7, 14, and 28 days. One-Way ANOVA was applied exclusively to the 28-day compressive strength data. The results indicate that increasing HDPE content reduces workability; however, concrete containing 10% HDPE maintains acceptable workability. At 28 days, the mixture with 10% HDPE achieved the highest compressive strength and showed a statistically significant improvement compared to the control. In contrast, a 15% HDPE replacement led to strength deterioration due to weak interfacial bonding. The novelty of this study lies in the statistically validated identification of an optimum HDPE replacement level in low-strength concrete under a constant superplasticizer dosage for non-structural application.